淡江大學機構典藏:Item 987654321/79680
English  |  正體中文  |  简体中文  |  Items with full text/Total items : 62805/95882 (66%)
Visitors : 3993379      Online Users : 298
RC Version 7.0 © Powered By DSPACE, MIT. Enhanced by NTU Library & TKU Library IR team.
Scope Tips:
  • please add "double quotation mark" for query phrases to get precise results
  • please goto advance search for comprehansive author search
  • Adv. Search
    HomeLoginUploadHelpAboutAdminister Goto mobile version
    Please use this identifier to cite or link to this item: https://tkuir.lib.tku.edu.tw/dspace/handle/987654321/79680


    Title: Preparation of compact Li-doped Y2Ti2O7 solid electrolyte
    Authors: Wen, L.C.;Hsieh, H.Y.;Lee, Y.H.;Chang, S.C.;Kao, H.-C.I.;Sheu, H.S.;Lin, I.N.;Chang, J.C.;Lee, M.C.;Lee, Y.S.
    Contributors: 淡江大學化學學系
    Keywords: (Y2 − xLix)Ti2O7 − x;Pyrochlore;Titanate;Li2O;Oxygen ion conductor
    Date: 2012-01-01
    Issue Date: 2013-01-08 17:14:58 (UTC+8)
    Publisher: Amsterdam: Elsevier BV * North-Holland
    Abstract: Three series of solid electrolytes were prepared with the nominal compositions of (Y2−xLi3x)Ti2O7 (Y3LT), (Y2−xLix)Ti2O7−x(YLT)and Y2−xTi2O7−3x/2 (YT) with x = 0.040 − 0.11. Comparing the unit cell a-axis of the YLT with that of YT, the latter is shorter with the same amount of x. This indicates a successful substitution of the Li ion into the Y site of Y2Ti2O7. However, both Y3LT and YLT have exactly the same unit cell a-axis length with the same amount of x so that the solid solution formed probably has the same formula, (Y2−xLix)Ti2O7−x, in which only one Li ion is substituted into the Y site. Extra Li2O added in the Y3LT is probably acting as a self flux to lower the melting point of the mixture. As a result, materials become more compact and grains grow bigger. One compound of Y3LT with x = 0.060 has a total conductivity of 4.3(4) × 10− 4 S⋅cm− 1 at 700 °C. Adding Li2O as a flux and carefully controlling the heat treatment history, compact sample of Y3LT with a relative density higher than 90% was obtained at a temperature as low as 1150 °C. Its ionic conductivity is comparable to one Y2Ti2O7 prepared at 1600 °C with a conductivity reported as 2.30 × 10− 4 S⋅cm− 1.
    Relation: Solid State Ionics 206, pp.39–44
    DOI: 10.1016/j.ssi.2011.10.021
    Appears in Collections:[Graduate Institute & Department of Chemistry] Journal Article

    Files in This Item:

    File Description SizeFormat
    index.html0KbHTML211View/Open
    SSI-12376-206-39-44-2012.pdf731KbAdobe PDF681View/Open

    All items in 機構典藏 are protected by copyright, with all rights reserved.


    DSpace Software Copyright © 2002-2004  MIT &  Hewlett-Packard  /   Enhanced by   NTU Library & TKU Library IR teams. Copyright ©   - Feedback